These are hardware-tuned starting settings for printing PVA on the Anycubic Kobra 2. The Anycubic Kobra 2 pairs a direct-drive extruder with a PTFE-lined hotend on an open frame, and tops out at 260°C hotend / 110°C bed. Against PVA's ideal range (185–215°C), that lands us at 200°C nozzle and 60°C bed. PVA dissolves in water for clean supports but is very moisture-sensitive and must stay dry.
Recommended PVA profile
| Hotend temperature | 200°C (tower 185–215°C) |
| Bed temperature | 60°C |
| Print speed | 42 mm/s |
| Retraction | 1 mm (direct drive) |
| Part cooling fan | 50% |
| Bed adhesion | Pairs with PLA; dissolves in water. |
| Nozzle | Brass 0.4 mm is fine |
| First layer speed | 15–21 mm/s; same bed temp, verify Z offset |
| Flow / extrusion multiplier | Start at 100%; calibrate flow before touching retraction |
| Drying | Strongly recommended — dry before printing if you hear popping or see inconsistent extrusion |
How PVA behaves
PVA property profile
Strength 30Flexibility 20
Heat resistance 20
Ease of printing 40
Durability 20
Calibration order
- Dry the spool if it shows moisture symptoms, then confirm the nozzle and build plate are clean.
- Print a temperature tower inside the 185–215°C range; pick the lowest temperature with strong layer bonding and clean overhangs.
- Calibrate flow, then pressure/linear advance if your firmware supports it.
- Tune retraction last — more distance is not always better, especially on the direct-drive Anycubic Kobra 2.
PVA brands & what to expect
PVA is a dissolvable support material that pairs with PLA. Brands differ in how cleanly they dissolve and how quickly they absorb moisture — and all of them are extremely moisture-sensitive.
Popular PVA brands: eSUN.
Common PVA problems on the Anycubic Kobra 2
| Symptom | Likely cause | Fix |
|---|---|---|
| Clogs / stringing | Absorbed moisture | Dry thoroughly and print from a sealed box. |
| Supports won’t dissolve cleanly | Water too cold / not enough time | Use warm water and agitation; allow more soak time. |
On the Anycubic Kobra 2 specifically: it is a fast machine, so if PVA looks rough, drop speed before blaming temperature — many "quality" issues here are really the hotend not keeping up with the flow.
FAQ
What temperature should I print PVA on the Anycubic Kobra 2?
What print speed works for PVA on the Anycubic Kobra 2?
What retraction should I use for PVA?
Do I need an enclosure for PVA on the Anycubic Kobra 2?
Do I need a hardened nozzle for PVA?
Reviewed 2026-08-18. See how these starting settings are calculated. Numbers are conservative starting points, not lab measurements.