HomeEasy / Everyday › Wood PLA

Wood PLA print settings

Wood PLA contains real wood fibres, so a 0.5 mm or hardened nozzle reduces clogging. A good universal starting point is 200°C hotend, 55°C bed and 45 mm/s, but the exact numbers depend on your printer — pick yours below.

190–215°C
Hotend range
55°C
Bed
Beginner
Difficulty

Wood PLA settings by printer

PrinterHotendBedSpeedRetr.
Creality Ender 3 V3 SE200°C55°C45 mm/s0.8 mm
Creality Ender 3 V2200°C55°C45 mm/s5 mm
Creality Ender 3 S1 Pro200°C55°C45 mm/s0.8 mm
Bambu Lab A1200°C55°C63 mm/s0.8 mm
Bambu Lab A1 mini200°C55°C63 mm/s0.8 mm
Bambu Lab P1P200°C55°C63 mm/s0.8 mm
Bambu Lab P1S200°C55°C63 mm/s0.8 mm
Bambu Lab X1 Carbon200°C55°C63 mm/s0.8 mm
Prusa MK4200°C55°C63 mm/s0.8 mm
Prusa MINI+200°C55°C45 mm/s5 mm
Anycubic Kobra 2200°C55°C63 mm/s0.8 mm
Sovol SV06200°C55°C45 mm/s0.8 mm
Creality K1200°C55°C63 mm/s0.8 mm
Creality K1 Max200°C55°C63 mm/s0.8 mm
Elegoo Neptune 4200°C55°C63 mm/s0.8 mm
Voron 2.4200°C55°C63 mm/s0.8 mm

Shop Wood PLA on Amazon →