Prusa’s in-house line, batch-tested with published diameter tolerance on every spool. This page collects recommended starting temperatures and settings for Prusament filament, then links each material to a full, hardware-aware profile for your specific printer.
Prusament temperatures at a glance: Prusament PLA ~215°C and PETG ~240°C are dialled in for Prusa machines out of the box.
Prusament settings by material
| Prusament filament | Hotend | Bed | Speed | Difficulty |
|---|---|---|---|---|
| Prusament PLA | 205°C | 60°C | 60 mm/s | Beginner |
| Prusament PETG | 240°C | 80°C | 50 mm/s | Intermediate |
| Prusament ASA | 250°C | 100°C | 45 mm/s | Advanced |
| Prusament Polycarbonate | 275°C | 110°C | 35 mm/s | Advanced |
💡 Tightest published tolerances; premium price but extremely consistent. Numbers are starting points — run a temperature tower per spool, since even one brand varies by colour and batch.
Pick your Prusament material
Prusament PLA205°C · bed 60°CPrusament PETG240°C · bed 80°CPrusament ASA250°C · bed 100°CPrusament Polycarbonate275°C · bed 110°C
Reviewed 2026-08-18. Prusament is an independent brand; FilamentPick is not affiliated. Settings are conservative starting points.