Hatchbox PLA is happy at 200–210°C; the wide colour range prints consistently. Below is a safe starting profile for Hatchbox TPU, plus the exact numbers capped to popular printers. TPU is flexible and prints best slow with a direct-drive extruder; Bowden setups must go very slow.
Quick answer: 225°C nozzle · 50°C bed · 25 mm/s · 1 mm retraction (direct drive). Tune per spool with a temperature tower.
225°
Hotend
50°
Bed
25
mm/s
60%
Part fan
What to expect from Hatchbox TPU
TPU comes in shore hardness grades (85A–95A most common). Softer TPU is harder to print, especially on Bowden machines. Brand matters less than shore rating and how slowly you’re willing to print.
🔎 Speed is everything with TPU — push it and the filament buckles instead of feeding. A direct-drive extruder transforms the experience; on a Bowden setup you’re limited to a crawl.
Hatchbox TPU on popular printers
| Printer | Hotend | Bed | Speed |
|---|---|---|---|
| Creality Ender 3 V3 SE | 225°C | 50°C | 25 mm/s |
| Creality Ender 3 V2 | 225°C | 50°C | 20 mm/s |
| Creality Ender 3 S1 Pro | 225°C | 50°C | 25 mm/s |
| Bambu Lab A1 | 225°C | 50°C | 25 mm/s |
| Bambu Lab A1 mini | 225°C | 50°C | 25 mm/s |
| Bambu Lab P1P | 225°C | 50°C | 25 mm/s |
| Bambu Lab P1S | 225°C | 50°C | 25 mm/s |
| Bambu Lab X1 Carbon | 225°C | 50°C | 25 mm/s |
| Prusa MK4 | 225°C | 50°C | 25 mm/s |
| Prusa MINI+ | 225°C | 50°C | 20 mm/s |
FAQ
What temperature should I print Hatchbox TPU at?
Start around 225°C hotend and 50°C bed, then run a temperature tower across 210–235°C. Hatchbox PLA is happy at 200–210°C; the wide colour range prints consistently.
Is Hatchbox TPU good quality?
Reliable, easy-to-find PLA that many tutorials are written around. As always, dry the spool if you see stringing or popping and calibrate flow before judging a brand.
Do I need to dry Hatchbox TPU?
Yes — TPU is moisture-sensitive regardless of brand. Dry it before printing if you hear popping or see whiskers.
Reviewed 2026-08-18. Independent guidance; not affiliated with Hatchbox.