HomePrusa MINI+ › Nylon (PA)

Nylon (PA) settings for the Prusa MINI+

Possible with tweaks

These are tuned starting settings for printing Nylon (PA) on the Prusa MINI+. The Prusa MINI+ has a Bowden extruder and an all-metal hotend, so we set the hotend to 260°C and the bed to 90°C. Nylon is extremely strong but soaks up moisture fast, so dry the spool before every print.

260°C
Hotend
90°C
Bed
40 mm/s
Speed
0%
Part fan

Recommended Nylon (PA) profile

Hotend temperature260°C (tower 240–280°C)
Bed temperature90°C
Print speed40 mm/s
Retraction6 mm (Bowden)
Part cooling fan0%
Bed adhesionGlue stick or PA-specific sheet; dry before printing.
NozzleBrass 0.4 mm is fine
DifficultyAdvanced
⚠️ Nylon (PA) warps without an enclosure and the Prusa MINI+ is open-frame. Block drafts, raise the bed temp, and add a brim; for tall parts an enclosure is strongly recommended.
💡 Best uses for Nylon (PA): gears, living hinges, tough parts.

Shop Nylon (PA) on Amazon →

FAQ

What temperature should I print Nylon (PA) on the Prusa MINI+?
Start at 260°C for the hotend and 90°C for the bed, then run a temperature tower across 240–270°C to dial in your exact filament brand.
What print speed works for Nylon (PA) on this printer?
Around 40 mm/s is a safe starting point on the Prusa MINI+.
What retraction should I use?
Use about 6 mm of retraction (Bowden setups need more). If you see stringing with Nylon (PA), raise retraction speed before distance and dry the filament.
Do I need an enclosure for Nylon (PA) on the Prusa MINI+?
Yes — Nylon (PA) really wants an enclosure and the Prusa MINI+ is open, so expect warping on large parts without one.