Home › Prusa MK4S › HIPS
HIPS settings for the Prusa MK4S
Workable with mods
⚡ Quick answer: Print HIPS on the Prusa MK4S at 240°C hotend, 100°C bed, 119 mm/s, 0% part-cooling fan and 0.8 mm retraction. Run a temperature tower to fine-tune your exact spool.
These are tuned starting settings for printing HIPS on the Prusa MK4S. The Prusa MK4S has a direct-drive extruder with an all-metal hotend, so we set the hotend to 240°C and the bed to 100°C. HIPS doubles as a light structural material and a limonene-dissolvable support for ABS.
240°C
Hotend
100°C
Bed
119 mm/s
Speed
0%
Part fan
⚠️ HIPS needs an enclosure and dissolves in limonene. The open Prusa MK4S works for small parts, but expect warping on anything large.
Recommended HIPS profile
| Hotend temperature | 240°C (tower 230–255°C) |
| Bed temperature | 100°C |
| Print speed | 119 mm/s |
| Retraction | 0.8 mm (direct drive) |
| Part cooling fan | 0% |
| Bed adhesion | ABS slurry or glue; enclosure needed. |
| Nozzle | Brass 0.4 mm |
| Difficulty | Advanced |
💡 Best uses for HIPS: dissolvable support for ABS (limonene) and light parts.
Troubleshooting HIPS on the Prusa MK4S
| Problem | Fix |
|---|---|
| Stringing or fine hairs | Dry HIPS before printing, drop the hotend a few degrees below 240°C, and raise retraction toward 1.2 mm. Damp filament is the No. 1 cause of stringing. |
| Poor first-layer adhesion | ABS slurry or glue; enclosure needed. Re-level the bed, set a slightly squished first layer, and wipe the sheet with IPA so it is grease-free. |
| Blobs, zits or rough walls | Slow the outer wall, enable coasting/wipe, and keep retraction near 0.8 mm. Keep the part-cooling fan low so layers bond and warping stays down. |
FAQ
- What temperature should I print HIPS on the Prusa MK4S?
- Start at 240°C for the hotend and 100°C for the bed, then run a temperature tower across 230–255°C to dial in your exact filament brand.
- What print speed works for HIPS on this printer?
- Around 119 mm/s is a safe starting point on the Prusa MK4S. It can go faster once the profile is tuned, but start conservative for clean walls.
- What retraction should I use?
- Use about 0.8 mm of retraction (direct drive needs very little). If you see stringing, raise retraction speed before distance and dry the filament.
- Do I need an enclosure for HIPS on the Prusa MK4S?
- Yes — HIPS needs an enclosure to avoid warping, and the Prusa MK4S is open, so add one or expect warping and cracking on larger parts.
Sources & how we tuned this
These settings are community-tested starting points, cross-checked against manufacturer guidance and trusted material references:
- Simplify3D — Ultimate 3D Printing Materials Guide
- All3DP — filament settings guides
- Prusa Knowledge Base
Last verified: 2026-07-17. Always run a temperature tower and a small calibration print for your exact spool.