These are hardware-tuned starting settings for printing PLA-CF on the Qidi Q1 Pro. The Qidi Q1 Pro pairs a direct-drive extruder with an all-metal hotend inside an enclosed chamber, and tops out at 350°C hotend / 120°C bed. Against PLA-CF's ideal range (205–230°C), that lands us at 215°C nozzle and 60°C bed. Carbon-fibre PLA is stiffer and matte but the fibres chew through brass nozzles fast.
Recommended PLA-CF profile
| Hotend temperature | 215°C (tower 205–230°C) |
| Bed temperature | 60°C |
| Print speed | 70 mm/s |
| Retraction | 0.8 mm (direct drive) |
| Part cooling fan | 100% |
| Bed adhesion | Easy like PLA; needs a hardened steel nozzle. |
| Nozzle | Hardened steel (this filament is abrasive) |
| First layer speed | 25–35 mm/s; same bed temp, verify Z offset |
| Flow / extrusion multiplier | Start at 100%; calibrate flow before touching retraction |
| Drying | Dry if the spool pops, strings unusually, or the surface looks rough |
How PLA-CF behaves
PLA-CF property profile
Strength 75Flexibility 5
Heat resistance 35
Ease of printing 65
Durability 50
Calibration order
- Dry the spool if it shows moisture symptoms, then confirm the nozzle and build plate are clean.
- Print a temperature tower inside the 205–230°C range; pick the lowest temperature with strong layer bonding and clean overhangs.
- Calibrate flow, then pressure/linear advance if your firmware supports it.
- Tune retraction last — more distance is not always better, especially on the direct-drive Qidi Q1 Pro.
PLA-CF brands & what to expect
Carbon-fibre PLA prints at PLA-like temperatures but the abrasive fibres are what matter — every brand will destroy a brass nozzle. A hardened steel nozzle is mandatory regardless of brand.
Popular PLA-CF brands: eSUN, Overture, Polymaker, Bambu Lab.
Common PLA-CF problems on the Qidi Q1 Pro
| Symptom | Likely cause | Fix |
|---|---|---|
| Rapid under-extrusion | Brass nozzle worn or clogging | Switch to hardened steel; a 0.5–0.6 mm nozzle helps. |
| Rough / fuzzy surface | Slightly cool or worn nozzle | Small temp bump; inspect the nozzle for wear. |
On the Qidi Q1 Pro specifically: fit a hardened nozzle before running much PLA-CF — the stock hotend still uses a brass nozzle that wears out fast on abrasive filament.
FAQ
What temperature should I print PLA-CF on the Qidi Q1 Pro?
What print speed works for PLA-CF on the Qidi Q1 Pro?
What retraction should I use for PLA-CF?
Do I need an enclosure for PLA-CF on the Qidi Q1 Pro?
Do I need a hardened nozzle for PLA-CF?
Reviewed 2026-08-18. See how these starting settings are calculated. Numbers are conservative starting points, not lab measurements.